MASTER BOND POLYMER ADHESIVE SUPREME 10HT/S
One Component, Heat Curing, High Purity Silver Conductive Epoxy Adhesive/Sealant Featuring
Both High Shear and High Peel Strength for Performance up to 400°F.
Meets NASA Outgassing Specifications.

Master Bond Polymer System Supreme 10HT/S represents a breakthrough in conductive epoxy technology, featuring a combination of high performance properties including both high shear and high peel strengths, low resistance, and exceptionally easy processing. This one component (no mix) high purity silver conductive system is formulated to cure at elevated temperatures, e.g. 45 minutes at 275°F-300°F or 1 hour at 250°F. Minimum curing temperature is 250°F. Tensile shear strengths in excess of 1200 psi and T-peel strengths in excess of 5 pli are readily obtained. Supreme 10HT/S produces its high performance bonds for service over the wide temperature range of 4K to 400°F, making it suitable for use in cryogenic applications. It offers superior resistance to high impact, thermal shock, vibration and stress fatigue cracking while maintaining the moisture, creep, corrosion and thermal resistance typical of epoxy resin adhesives. Supreme 10HT/S can be applied without sagging or dripping even on vertical surfaces. It is 100% reactive and does not contain any diluents or solvents, although it can be made thinner by adding 5 to 10% of acetone or xylene by weight.

Supreme 10HT/S forms tough, low resistance bonds that are resistant to many chemicals including water, oil, fuels and most organic solvents. The excellent electrical conductivity is fully retained even upon severe thermal cycling. Adhesion to metals, glass, ceramics, vulcanized rubbers and many plastics is superb. The cured system is also a superior thermal conductor. Supreme 10HT/S offers the convenience of a heat cure with no mixing prior to use. It cures to form high performance bonds that are well suited for difficult applications in the aerospace, electronic, electrical, computer, metalworking, appliance, automotive and chemical industries.

Click here to request additional information on this product




Contact Us Overview Products
by Type
Products
by Use
Packaging
Solutions
Ordering
& Sales
News Technical
Reference
Site
Map
Legal Notices & Credits © Copyright 1999-2009 Master Bond Inc., All Rights Reserved