This email was sent to (%email%)
  Unsubscribe at:  http://www.masterbond.com/phplist/?p=unsubscribe&id=2
  Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2 
----------------------------------
The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=su46ht-2.
----------------------------------
  FOR IMMEDIATE RELEASE
Heat Resistant Epoxy Adhesive for 
High Performance Structural Bonding
HACKENSACK, NJ - Apr 8, 2010 - For outstanding, high performance bonding strength to both similar and dissimilar substrates, Master Bond Polymer Supreme 46HT-2 was developed. This two component adhesive features high temperature resistance along with superior toughness and strength. It has excellent durability, thermal cycling and shock capabilities, as well as superb electrical insulation properties.
With a balance of superior peel and shear strength properties, Supreme 46HT-2 is suitable for applications where long term exposure to wide temperature ranges between -100°F and +500°F is required. It is used extensively in aerospace, electronic, metalworking, transportation, appliance and chemical/oil processing applications.
With a mixing ratio of 100 to 30, it cures at elevated temperatures with a minimum 250°F required for cure. Moreover, product properties are relatively unaffected by small changes in mix ratio. There is also a non-drip version available called Supreme 46HT-2ND2 that will not flow during cure. It is available for purchase in half-pint, pint, quart, one gallon and five gallon container kits.
CONTACT:
  James Brenner, Marketing Manager
  Email: jbrenner@masterbond.com
  Tel: 201-343-8983
  Fax: 201-343-2132
MASTER BOND INC.
  154 Hobart Street
  Hackensack, NJ 07601-3922