This email was sent to (%email%)
  Unsubscribe at:  http://www.masterbond.com/phplist/?p=unsubscribe&id=2
  Subscribe at: http://www.masterbond.com/phplist/?p=subscribe&id=2 
----------------------------------
The following is a news release from Master Bond Inc. You have received it because you are listed as an editor for your publication.
Attached to this email is a low resolution version of the photograph that is included in the press kit for this product.
High resolution versions of this image and files with the body text of this release are available at http://www.masterbond.com/mbnr.html?nr=ep42ht-2fg.
----------------------------------
  FOR IMMEDIATE RELEASE
New, Versatile Food Grade Epoxy Resists High Temperatures & Harsh Conditions 
Tested and Certified to Meet FDA CFR 175.300
HACKENSACK, NJ - May 19, 2011 - Master Bond is pleased to announce the release of EP42HT-2FG, a new food grade epoxy system. EP42HT-2FG has been independently tested and certified by a leading national laboratory to meet the stringent requirements of FDA CFR 175.300. It also was toxicologically evaluated to meet the NSF/ANSI 51.4.1 (2009) standard for food equipment materials.
Food grade certified epoxy EP42HT-2FG may be used across a wide variety of applications in the food industry, such as bonding and sealing metals, plastics, rubbers and other substrates, commonly found on food service equipment. Featuring high resistance to chemicals and many solvents, along with boiling water, fats and oils, it may be readily used as a coating for storage tanks, bins, hoppers, and other containment vessels. Capable of withstanding extreme conditions over the wide service temperature range of -60°F to +450°F (FDA certification done at the temperatures specified in the test protocol), EP42HT-2FG resists steam, radiation and frozen storage conditions.
With a volume resistivity of over 1014 ohm-cm, EP42HT-2FG also serves as a potting and encapsulation compound for electronic components and devices. It has a low viscosity of 55,000-110,000 cps for Part A and 75-130 cps for Part B at room temperature. This adhesive has a tensile strength greater than 12,000 psi and a tensile lap shear strength exceeding 2,000 psi at 75°F.
This two part epoxy offers easy handling with an open time of 45-75 minutes for a 100 gram mass at 75°F. EP42HT-2FG has convenient color coding (Part A is clear and Part B is amber) for its 100:30 mix ratio by weight. The recommended cure is 3-4 hours at 150-200°F. Alternatively, it can be cured at room temperature overnight followed by a 2-3 hour cure at 150-200°F.
EP42HT-2FG is available for use in half-pint, pint, quart, gallon and five gallon containers. It has a shelf life of one year when stored at room temperature in its original unopened containers.
Master Bond High Two Component Epoxy Systems
Master Bond’s EP42HT-2FG has superior heat resistance and approval for use in demanding food grade applications. Read more about Master Bond’s Two Component Epoxy Systems at http://www.masterbond.com/lp/tabs/tp_byt_2ptepoxy.html or contact Technical Support by phone at +1-201-343-8983, by fax at +1-201-343-2132 or by e-mail at techinfo@masterbond.com.
CONTACT:
  James Brenner, Marketing Manager
  Email: jbrenner@masterbond.com
  Tel: 201-343-8983
  Fax: 201-343-2132
MASTER BOND INC.
  154 Hobart Street
  Hackensack, NJ 07601-3922
  Web: www.masterbond.com
# # #