  The following is a news release from Master Bond Inc. You have received it  because you are listed as an editor for your publication.
  Attached to this email is a low resolution version of the photograph that is  included in the press kit for this product.
  High resolution version of this image and files with the body text of this  release in Word, HTML and text formats are available at http://www.masterbond.com/newsrelease/ep21ndfg.
  -----------------------------------------------------------------
Featuring a thick paste consistency, Master Bond EP21NDFG bonds well to a variety of substrates including metals, composites, glass, ceramics and many types of rubbers and plastics. Unlike many high viscosity systems, EP21NDFG is truly non-drip and will not run or sag, even when applied to vertical surfaces. It produces high strength, durable bonds that resist thermal cycling as well as chemicals including water, oils, fuels, acids, bases and salts.
EP21NDFG is a two component, room temperature curing epoxy that has a non-critical one to one mix ratio by weight or volume. It also has the unusual characteristic of being able to adjust the properties of the cured system by altering the mix ratio. Adding more of Part A (e.g. 2:1 mix ratio) will give a more rigid cure, while adding more of Part B (e.g. 1:2 mix ratio) gives a more forgiving cure.
Once cured, EP21NDFG is an electrically insulative system. It is serviceable over the wide temperature range of -60°F to +250°F. The color of both Parts A and Part B is amber, although, a wide variety of additional color choices are also available. Passing FDA Section 175.105 tests, EP21NDFG is primarily used in food equipment applications where there is an indirect exposure to food and related products. This epoxy is available in standard packaging options ranging from ½ pint to 5 gallon container kits.
Master Bond EP21NDFG is an easy to handle, non-drip, high strength epoxy for indirect food applications. Read more about Master Bond’s high strength systems at http://www.masterbond.com/properties/strength-properties-epoxy-compounds or contact Tech Support. Phone: +1-201-343-8983 Fax: +1-201-343-2132 Email: technical@masterbond.com.
Note to Editors:
For a full product description,  please visit: http://www.masterbond.com/tds/ep21ndfg 
  Check out product videos on our  YouTube channel: http://www.youtube.com/user/MasterBondVideo
You can embed any of our videos on your website.
CONTACT
  James Brenner, Marketing Manager
  Email: jbrenner@masterbond.com
  Tel: +1-201-343-8983
  Fax: +1-201-343-2132
MASTER BOND INC
  154 Hobart Street
  Hackensack, NJ 07601-3922
  Web: www.masterbond.com
# # #