One part UV system for high performance bonding, sealing, coating and encapsulation
Key Features
- Low viscosity
- Excellent optical clarity
- Good bond strength with excellent physical properties
- Low shrinkage upon cure
Product Description
Master Bond UV15-7HP is a one component, UV curable polymer system for high performance bonding, sealing, coating and encapsulation. Its most salient features include superior physical strength properties, low shrinkage upon curing and good optical clarity. This system bonds well to a wide variety of substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of polyester films. It is 100% reactive and does not contain any solvents or diluents. UV15-7HP offers very good chemical resistance to water, fuels and many solvents. The UV cured polymeric material can be employed over the wide service temperature range of -80°F to +300°F. UV15-7HP exhibits an excellent combination of properties including outstanding toughness, electrical insulation and withstands thermal cycling.
Master Bond UV15-7HP system is not oxygen inhibited and generally cures in 15-45 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections up to 1/8 inch. However when bonding, sections of a few thousandths of an inch are more than adequate. This system is widely used in optical, fiber-optic, electronic, laser, microelectronic and semiconductor applications.
Product Advantages
- Fast cure upon exposure to a UV light source
- No oxygen inhibition
- Superb electrical insulator
- Exceptional bond strength with good toughness
- Good dimensional stability
- Outstanding optical clarity and light transmission
Industrial Certifications
Packaging
UV15-7HP is available is various sizes and units to accommodate customer's needs.
 
			      