Benefits of Sodium Silicate Systems
- Water-based systems
- Environmentally friendly
- Room temperature or heat curable
- Superior dimensional stability
- Moisture resistant
- Outstanding thermal stability
Electrically insulative and electrically conductive grades are available for use.
Most Popular Sodium Silicate System
|   | MB600 Environmentally safe, water soluble, one part system. Thermal stability up to +1,500°F. Outstanding strength, dimensional stability and electrical insulation properties. Completely odorless, non-toxic and non-flammable. Cures obtained at moderately elevated temperatures. | 
|   | MB600S Aqueous based sodium silicate system. One component, silver filled formulation. Highly effective moisture barrier. Bonds well to a wide variety of substrates. Temperature resistance up to 700°F. Excellent shielding effectiveness. Simple, safe handling. | 
 
			      