One component, moderate viscosity, UV curable system meets NASA low outgassing
Key Features
- Excellent physical strength properties
- High dimensional stability
- Superior temperature and chemical resistance
- Not oxygen inhibited
Product Description
Master Bond UV24TKLO is a one part, modified epoxy acrylate UV curable system for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-595. It has outstanding resistance to chemicals, as described in part below. Upon curing, it should be noted that UV24TKLO is slightly translucent. The best wavelengths for curing are 320-365 nm and the energy requirement is 10-40 milliwatts per cm2. This UV system is not oxygen inhibited.
UV24TKLO has superb physical strength and electrical insulation properties. The service temperature range is -60°F to +400°F and its Tg is 120-130°C. The UV24TKLO can be cured in thicker sections, up to 1/16 of an inch and can be easily “layered” to higher levels. Most notable is that it passes the NASA low outgassing test, which enables it to be used in a wide array of applications where that property is a requirement. In order to optimize cured properties, post curing at 80-110°C for 2-4 hours is strongly recommended, if possible. Even heating at a lower temperature will enhance properties.
Product Advantages
- One component, no mixing required
- Not oxygen inhibited
- Outstanding physical strength properties
- Reliable electrical insulator
- Relatively high Tg
Industrial Certifications
Packaging
UV24TKLO is available is various sizes and units to accommodate customer's needs.
 
			      