In several published research articles, patents, and manufacturers’ specifications, scientists and engineers have identified EP21TDCS-LO for use in their applications due to its unparalleled performance in one or more areas. The table below highlights two research applications that use Master Bond EP21TDCS-LO.
Durable, high strength two component epoxy for bonding and sealing
Key Features
- Low volume resistivity
- Outstanding toughness
- Cryogenically serviceable
- Passes ASTM E595 for NASA low outgassing
Product Description
Master Bond EP21TDCS-LO is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing. It is formulated to cure at room temperature or more rapidly at elevated temperatures. The optimum cure schedule is overnight at room temperature followed by 2-3 hours at 135-165°F. Unlike many two part silver conductive epoxy systems, EP21TDCS-LO has a one to one mix ratio by weight or volume. Both parts A and B are paste consistency and after mixing, the system is essentially nondrip. It is 100% reactive and does not contain any diluents or solvents. After curing, the system has several attractive features including very low volume resistivity.
EP21TDCS-LO bonds well to a wide variety of substrates such as metals, glass, composites, ceramics, as well as many plastics. It is a toughened system which allows it to withstand rigorous thermal cycling and shock. This silver conductive epoxy has a service temperature range extending from 4K to +275°F. It is NASA low outgassing tested and approved. EP21TDCS-LO has been successfully used in sophisticated aerospace, optical, electro-optic, semiconductor, specialty OEM and related applications.
For convenient handling, EP21TDCS-LO is available in premixed and frozen syringes.
Product Advantages
- Easy to use mix ratio of 1 to 1 by weight or volume
- Paste consistency
- Cures at ambient or elevated temperatures
- Highly electrically and thermally conductive
- Excellent toughness
- Resists thermal cycling
- Passes NASA low outgassing testing
Product Citation
EP21TDCS-LO was cited in a paper titled "Ultrahigh Vacuum Cryostat System for Extended Low Temperature Space Environment Testing" by Justin Dekany, Robert H. Johnson (Utah State University), Gregory Wilson, Amberly Evans, JR Dennison (Utah State University). For more information click here.
Industrial Certifications
Packaging
EP21TDCS-LO is available is various sizes and units to accommodate customer's needs.
 
			      