Two component epoxy system featuring the special combination of fast setup times and high temperature resistance
Key Features
- Convenient handling
- Good physical strength properties
- Meets NASA low outgassing specifications
- Cures rapidly even in small masses
Product Description
Master Bond EP65HT is a specialty type system that features the unusual combination of ultra fast curing and high temperature resistance. While typical fast setting epoxies normally possess glass transition temperatures (Tg) below 85°C, EP65HT has an exceptional Tg of approximately 125°C. In addition, unlike typical fast cure epoxies, EP65HT retains fast setup times even when mixed in relatively small masses. EP65HT normally will setup in 9-12 minutes in 10-20 gram masses. A full cure generally occurs within 12-18 hours with high tensile shear strengths of over 1,200 psi. This system offers good physical properties, including low shrinkage upon cure, excellent dimensional stability and a high tensile modulus. The service temperature range is -60°F to +400°F. EP65HT offers sound electrical insulating properties and a useful chemical resistance profile. EP65HT fully meets the NASA low outgassing specifications and is particularly well suited for vacuum applications.
EP65HT bonds well to a wide variety of substrates including metals, glass, ceramics, vulcanized rubbers and many plastics. Dispensing EP65HT can be greatly facilitated by utilizing a dispensing gun capable of mixing fast setting materials with a ten to one mix ratio. This system is 100% reactive and does not contain any solvents. Part A is clear, and Part B is dark brown in color. It is especially useful for both prototyping and manufacturing in the aerospace, electronic, optical, electro-optical, vacuum related as well as specialty OEM applications where the special blend of fast curing and high temperature resistance is desirable.
Product Advantages
- Ultra fast setting and curing even in small masses; very short fixturing time
- Exceptionally high heat resistance
- Good physical strength properties
- Superior electrical insulation properties
- Available with convenient dispensing gun
- NASA low outgassing certified
Industrial Certifications
Packaging
EP65HT is available is various sizes and units to accommodate customer's needs.
 
			      