Master Bond UV22DC80-1 was used in a prototype concentrator photovoltaic (PV) system by researchers.
Two part high performance epoxy for bonding, sealing, coating and casting
Key Features
- Long working life
- Service temperature range from -100°F to +500°F
- Resists prolonged exposure to hostile environments
- Withstands 1,000 hours 85°C/85% RH
Product Description
Master Bond EP46HT-2 is a versatile two component epoxy system that can be used for bonding, sealing, coating and casting. It is most prominent for its temperature resistance along with the capability of withstanding aggressive chemicals. Its service temperature range extends from -100°F to +550°F. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly and requires a minimum curing temperature of 250°F; although a variety of cure schedules are possible. It should be noted that the mix ratio is a very forgiving 100 to 30-35 parts by weight. Upon curing, EP46HT-2 has a wide array of impressive physical and mechanical properties. It bonds well to a variety of substrates including metals, composites, ceramics, glass, rubbers and many plastics. One of the more noteworthy attributes of this system is its chemical resistance profile, which includes the ability to withstand many acids, bases, oils, fuels, hydrocarbons and solvents. It is also a very good electrical insulator. Unlike the EP46HT-1 product series, this line is not exothermic and can be used for potting and encapsulation. The color of Part A is clear; the color of Part B is brown. Master Bond EP46HT-2 is primarily used in specialty aerospace, electronic, petrochemical and OEM applications where high temperature resistance and the ability to withstand hostile chemicals is desirable.
Product Advantages
- Very forgiving mix ratio
- Long open time at room temperature
- Excellent thermal stability
- Capable of withstanding aggressive chemicals
- Good physical strength properties
Industrial Certifications
Packaging