One part epoxy, Supreme 18TC, contains a blend of special thermally conductive fillers allowing it to maintain outstanding heat transfer capabilities.
This smooth paste system can be applied in bond lines as thin as 10-15 microns. Supreme 18TC features ultra low thermal resistance and meets NASA low outgassing specifications.