                              | Having trouble viewing images? View email in browser |  
                  |  |  
            | 
                
                  | 
                      
                        |  |  
                        |  |  
                        |  |  
                        | 
                            
                            
                              | EP30HT-LO: Utilized by NASA to bond components in lunar exploration vehicles |  
                              |  |  
                              | Learn how researchers at the NASA Glenn Research Center doped Master Bond EP30HT-LO epoxy with silver and then used it to bond titanium thermosyphons to a graphite substrate, as well as graphite/isocyanate composite cooling fins to successfully investigate the production of non-condensable gases inside the thermosyphons. |  
                              |  |  
                              |  |  
                              |  |  |  
                        |  |  |  |  
            |  |  |  
    
      | 
          
            | 
                
                  | 
                      
                        |  |  
                        | 
                            
                              
                                | 
                                    
                                    
                                      | Two Part Epoxy EP30HT-LO |  
                                      |  |  
                                      | EP30HT-LO is a moderate viscosity, two component epoxy system highlighted by high temperature resistance and optical clarity. |  
                                      |  |  
                                      |  |  
                                      |  |  |  |  |  
                  |  |  |  |  
    
      |  |  
      | 
          
            |  |  
            | 
 
                